Research Article
[Retracted] Study of Surface Roughness of Cutting Isothermally Hardened Ductile Iron in Tosa Knife Forging Technique Based on Intelligent Calculation
Table 2
Mechanical properties of ADI materials.
| Group no. | Isothermal temperature () | Tensile strength () | Elongation (%) | Fracture condition | Hardness |
| ADI1 | 300 | 1385 | 1.80 | Normal | 45.8HRC | ADI2 | 350 | 1390 | 2.80 | Normal | 41.5HRC | ADI3 | 400 | 1080 | 1.55 | Normal | 37.8HRC |
|
|