Research Article
Post-Fracture Stiffness and Residual Capacity Assessment of Film-Retrofitted Monolithic Glass Elements by Frequency Change
Figure 6
Full 3D solid numerical model (ABAQUS): (a) detail of crack region (photo by ©C. Bedon) and (b) typical fundamental vibration shape (with hidden mesh pattern).
(a) |
(b) |