Research Article
Influence of the Microstructure and Silver Content on Degradation, Cytocompatibility, and Antibacterial Properties of Magnesium-Silver Alloys In Vitro
Table 3
Calculated concentrations of elements in the extracts of extruded pure Mg and Mg-Ag alloys.
| Extracts | Dilution | Concentration (mg/L) | Mg | Ca | Ag |
| Pure Mg (extrusion) | 1 | 1210 | 27 | <0.1 | 1/5 | 258 | 65.4 | <0.1 | 1/10 | 139 | 70.2 | <0.1 | Mg-6Ag (extrusion) | 1 | 1280 | 26 | 1.2 | 1/5 | 272 | 65.2 | 0.24 | 1/10 | 146 | 70.1 | 0.12 | Mg-6Ag (T4) | 1 | 1010 | 17 | 0.31 | 1/5 | 218.8 | 62.6 | 0.062 | 1/10 | 119.9 | 68.3 | 0.031 | Mg-8Ag (extrusion) | 1 | 1150 | 25 | 104 | 1/5 | 246 | 65 | 20.8 | 1/10 | 133 | 70 | 10.4 | Mg-8Ag (T4) | 1 | 930 | 15 | 0.64 | 1/5 | 202.8 | 62.2 | 0.128 | 1/10 | 111.9 | 68.1 | 0.064 | Cell culture medium (CCM) | 20 | 75 | <0.1 |
|
|