Research Article
Nanoscale Mechanical Properties of Nanoindented Ni48.8Mn27.2Ga24 Ferromagnetic Shape Memory Thin Film
Figure 3
Nanoindentation curves of the thin film annealed at 723 K, 773 K, and 823 K for 1 hour under a maximum load of 9 mN at room temperature.