Fractographic Analysis of Brinar 400 and Brinar 500 Steels in Impact Testing
Figure 21
Fracture surfaces of longitudinal Brinar 400 specimens in normalized condition after testing at +20°C: (a) under-notch zone; (b) central zone; (c) final-fracture zone. Unetched; SEM.
(a) |
(b) |
(c) |