Research Article

Fractographic Analysis of Brinar 400 and Brinar 500 Steels in Impact Testing

Figure 23

Fracture surfaces of transverse Brinar 400 specimens in normalized condition after testing at +20°C: (a) under-notch zone; (b) central zone; (c) final-fracture zone. Unetched; SEM.
(a)
(b)
(c)