Research Article

Physical Properties and Precipitate Microstructures of Cu-Hf Alloys at Different Processing Stages

Figure 10

Optical micrograph of the solid-solution-treated Cu-Hf alloy: (a) Cu-0.15Hf, (b) Cu-0.4Hf, and (c) Cu-0.9Hf.
(a)
(b)
(c)