Research Article
Structural and Kinetic Hydrogen Sorption Properties of Zr0.8Ti0.2Co Alloy Prepared by Ball Milling
Table 1
Rietveld refinement results of XRD patterns of
samples after ball milling for different time.
| System | Ball milling time/hour | Space group | Lattice parameters of major constituent phase (ZrCo phase)/Å | Cell volume of major constituent phase (ZrCo phase)/Å3 |
| ZrCo [13] | 0 | Pm-3m | 3.1957 | 32.64 | | 0 | Pm-3m | 3.1638 | 31.67 | 2 | 3.1587 | 31.55 | 4 | 3.1574 | 31.48 | 6 | 3.1555 | 31.42 | 8 | 3.1534 | 31.35 |
|
|