EIS parameters obtained for corrosion of Ni, Ni-3, Ni-6, and Ni-9 g/L of AlN coating after being tested in 3.5 wt% NaCl aqueous solution at open circuit potential within a frequency range of 0.1 to 100 kHz at 25°C.

Sample, KΩ·cm2, Ω·cm2CPE2, (cm−2) ()

Ni3.75318.540.858
Ni-AlN-3 g/L6.01221.930.913
Ni-AlN-6 g/L7.7622.020.875
Ni-AlN-9 g/L9.62123.870.872