Research Article
Effects of Hydrogen Contents on Oxidation Behavior of Alloy 690TT and Associated Boron Accumulation within Oxides in High-Temperature Water
Figure 4
Normalization of the oxide films formed on Alloy 690TT in simulated primary water with different DH contents at 330°C for 500 h: (a) 0.4494 mg/kg, (b) 3.1458 mg/kg, (c) 4.4940 mg/kg, and (d) 5.8422 mg/kg.
(a) |
(b) |
(c) |
(d) |