Review Article
Biodegradable Magnesium Alloys Developed as Bone Repair Materials: A Review
Figure 6
SEM images of β-tricalcium phosphate-coated AZ31, naked AZ31, and Ti-6Al-4V alloy rod samples after implantation for 1, 4, and 12 weeks. Scale bar = 5 μm [59].