Research Article
Corrosion Resistance of Waterborne Epoxy Resin Coating Cross-Linked by Modified Tetrabutyl Titanate
Figure 6
Appearance of epoxy resin, ET3, ET6, and ET9 coating before (a–d) and after (e–h) 30 days of immersion in 3.5% NaCl solution.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |
(g) |
(h) |