Research Article

Effect of Diamond Surface Pretreatment and Content on the Microstructure and Mechanical and Oxidation Behaviour of NiAl/Fe-Based Alloys

Figure 11

Cross-section image of the oxide film of the NiAl/Fe-based alloy after oxidation for 25 h: (a) NiAl/Fe-based alloys with 0 wt.% diamond; (b) NiAl/Fe-based alloys with 10 wt.% diamond.
(a)
(b)