Research Article
Surface Characterization and Corrosion Resistance of Biomedical AZ31 Mg Alloy Treated by Microarc Fluorination
Table 2
Sample code name and the process of preparing MAF treatment.
| Code | Surface treatment | Processing time |
| AZ31 | None | None | MAF100 | Immersed in 46% hydrofluoric acid at DC and constant voltage of 100 V | 30s | MAF150 | Immersed in 46% hydrofluoric acid at DC and constant voltage of 150 V | 30s | MAF200 | Immersed in 46% hydrofluoric acid at DC and constant voltage of 200 V | 30s | MAF250 | Immersed in 46% hydrofluoric acid at DC and constant voltage of 250 V | 30s | MAF300 | Immersed in 46% hydrofluoric acid at DC and constant voltage of 300 V | 30s |
|
|