Research Article

Evaluation of the Bond Strengths between Dental Porcelain and Cobalt-Chromium Metal Frameworks Manufactured with Different Techniques after the Thermal Aging Process

Table 5

Descriptive statistics and one-way ANOVA test result of binding strengths (MPa) based on different production methods.

Mean (SD)MinMax value

Casting3042.41 (4.87)31.9855.03
CAD/CAM (milling)3052.86 (7.60)37.0168.110.0001
EOS (laser sintering)3043.15 (1.92)40.0646.92
Concept (laser sintering)3044.46 (2.38)39.2349.05

SD: standard deviation; Min: minimum; Max: maximum.