Research Article
Fabrication of Core-Shell PEI/pBMP2-PLGA Electrospun Scaffold for Gene Delivery to Periodontal Ligament Stem Cells
Table 2
Mechanical properties of the three groups of electrospun scaffolds (mean
standard deviation).
| ā | Core-shell scaffold | Single axial scaffold | PLGA scaffolds |
| Ultimate strength (MPa) | 3.51 0.5 | 2.57 0.31 | 4.60 0.46 | Elastic modulus (MPa) | 11.34 3.22 | 10.23 4.08 | 15.57 0.96 | Ultimate strain (%) | 29.87 3.98 | 26.45 2.53 | 35.46 3.92 |
|
|