Research Article

Osteogenic Differentiation of hDPSCs on Biogenic Bone Apatite Thin Films

Table 1

Root mean square (RMS) roughness and wettability of deposited films and glass substrate.

SampleRMS at 10 μm2 (nm)Contact angle (°)

HA_AD140 ± 1957.9 ± 2.8
HA_HT173 ± 948.8 ± 3.1
BAp_AD243 ± 4647.6 ± 1.4
BAp_HT209 ± 2436.2 ± 0.9