Research Article
Knitted 3D Scaffolds of Polybutylene Succinate Support Human Mesenchymal Stem Cell Growth and Osteogenesis
Figure 2
Material characterization. (a) Crystallinity of the materials after 0, 1, 2, 3, and 4 weeks of hydrolysis. (b) Inherent viscosity after 0, 1, 2, 3, and 4 weeks of hydrolysis; . (c) Toughness of the materials after 0, 1, 2, 3, and 4 weeks of hydrolysis; . (d) Strain at break after 0, 1, 2, 3, and 4 weeks of hydrolysis; . between the indicated material () and PLA at the same time point.
(a) |
(b) |
(c) |
(d) |