Experimental results of the brick samples fired at 900°C.

Mix codeWeight loss
(%)
Bulk density (g/cm3)Porosity (%)Water absorption (%)Bending strength (MPa)Compressive strength (MPa)

06.761.6833.916.514.134.9
10F5.881.8334.616.113.532.0
20F5.071.8638.218.17.129.8
30F4.691.9038.617.49.227.5
10Z7.541.6537.420.38.222.3
20Z8.171.5639.322.46.519.4