Research Article

The Forecasting of Corrosion Damage of Structural Materials during Dry Long-Term Storage of RD BN-350 SNF with CC-19 SFA

Table 2

The results of processing the experimental curves of oxidation kinetics.

Annealing temperature, °СSampleEmpirical formula

600Irradiated FA jacketG = 0.3708·τ0,044(1)
Nonirradiated FA jacketG = 0.1758·τ0,0934(2)
Nonirradiated fuel element claddingG = 0.2937·τ0,181(3)

400Irradiated FA jacketG = 0.0085·τ0,318(4)
Nonirradiated FA jacketG = 0.0039·τ0,3393(5)
Nonirradiated fuel element claddingG = 0.0013·τ0,3284(6)