The results of processing experimental curves of oxidation kinetics.
| Annealing temperature, °С | Sample | Empirical formula |
| 550 | Irradiated FA jacket | G = 0.0664·τ0,181 | (7) | Nonirradiated FA jacket | G = 0.0696·τ0,227 | (8) | Nonirradiated fuel element cladding | G = 0.0522·τ0,222 | (9) |
| 400 | Irradiated FA jacket | G = 2·10−6·τ + 0,0138 | (10) | Nonirradiated FA jacket | G = 5·10−6·τ + 0,0352 | (11) | Nonirradiated fuel element cladding | G = 10·10−6·τ + 0,0388 | (12) |