Research Article
A Fracture Criterion for Prediction of Fracture Initiation of Metal Materials at Various Stress States for Nuclear Waste Storage
Figure 5
SEM images of fracture surfaces for QT400 nodular cast iron in combined tension-torsion tests with different tension-torsion ratios on the fracture surface of the specimen with tension-torsion ratio (a) P/T = 0.0, (b) P/T = 0.17, (c) P/T = 0.38, and (d) P/T = 0.72.
(a) |
(b) |
(c) |
(d) |