The experimental data points of QT400-15 nodular cast iron in combined tension-torsion tests.

P/T0.00.170.380.72
(kN)0.015.525.334.442.1
(N·m)115.590.366.747.20.0
(MPa)588.5568.6555.0544.4536.6
(MPa)00000
(MPa)−588.5−371.6−214.4−106.20.0
0.00.080.160.240.33
(°)423832220
(°)453933240