The Influence of Radiation on Confinement Properties of Nuclear Waste Glasses

Table 3

Composition of borosilicate glasses produced by AREVA at La Hague (France).

OxidesContents, wt.%OxideContents, wt.%

SiO242.4–51.7Cr2O3<0.6
B2O312.4–16.5P2O5<1
Al2O33.6–6.6Li2O1.6–2.4
Na2O8.1–11.0ZnO2.2–2.8
CaO3.5–4.8Fission products + miscellaneous7.5–18.5
Fe2O3<4.5
NiO<0.5Actinide oxides0.6