Research Article
Investigation of Oxidation and Counter-Oxidation in a One-Quarter Circular Geometry due to Shadow Corrosion
Figure 6
Comparison of oxide thickness profiles obtained under the same working conditions with platinum as CE (a) for Zry-2 in a plane geometry [7] and (b) for Zry-2 in a ¼ circular geometry.
(a) |
(b) |