Variation of oxide thickness as a function of the degree of dissociation (α) for an arbitrary smooth surface of Zry-2.

αOxide thickness (µm) at various electrode distances d
d = 0.08 mmd = 0.5 mmd = 1.0 mmd = 2.0 mmd = 5.0 mm

019.9919.9818.5410.794.16
0.119.9919.9919.6512.815.03
0.219.9919.9919.9014.645.87
0.519.9919.9919.9918.558.23
119.9919.9919.9919.9311.72