Crack length evaluation with the wave fields obtained in (a) the free plate (single scan), (b) the water-immersed plate (10 times scans), and (c) the glycerin-immersed plate (10 times scans).
895693.fig.0010a
(a)
895693.fig.0010b
(b)
895693.fig.0010c
(c)