Shock and Vibration / 2019 / Article / Tab 7 / Research Article
Dynamic Compressive and Tensile Characteristics of a New Type of Ultra-High-Molecular Weight Polyethylene (UHMWPE) and Polyvinyl Alcohol (PVA) Fibers Reinforced Concrete Table 7 Performance parameters of fiber concrete of different groups under different strain rates.
Group no. Air pressure (MPa) Strain rate (sā1 ) Dynamic tensile strength (MPa) Static compressive strength (MPa) DIF 0 0.20 7.84 8.21 3.84 2.14 0.25 12.43 11.13 2.90 0.30 18.32 13.54 3.53 0.35 24.25 15.43 4.02 0.40 29.67 17.05 4.14 P-0.6 0.20 7.66 8.78 4.01 2.19 0.25 12.24 11.92 2.97 0.30 17.83 14.52 3.62 0.35 23.76 16.58 4.13 0.40 29.27 18.37 4.58 U-0.6 0.20 7.42 8.97 4.06 2.21 0.25 12.08 12.18 3.00 0.30 17.58 14.84 3.66 0.35 23.49 16.95 4.17 0.40 28.96 18.77 4.62 P-1.2 0.20 7.26 9.17 4.09 2.24 0.25 11.95 12.46 3.05 0.30 17.42 15.19 3.71 0.35 23.20 17.36 4.24 0.40 28.72 19.24 4.70 U-1.2 0.20 7.15 9.44 4.14 2.28 0.25 11.83 12.82 3.10 0.30 17.27 15.63 3.78 0.35 22.98 17.86 4.31 0.40 28.43 19.78 4.78 P-1.8 0.20 7.09 9.52 4.16 2.29 0.25 11.71 12.92 3.11 0.30 17.13 15.73 3.78 0.35 22.82 17.84 4.29 0.40 28.21 19.69 4.73 U-1.8 0.20 6.97 9.69 4.20 2.31 0.25 11.48 13.18 3.14 0.30 16.74 16.10 3.83 0.35 22.37 18.39 4.38 0.40 27.62 20.38 4.85 P-2.4 0.20 6.89 9.61 4.21 2.28 0.25 11.36 13.07 3.10 0.30 16.58 15.95 3.79 0.35 22.13 18.24 4.33 0.40 27.35 20.19 4.80 U-2.4 0.20 6.75 9.87 4.26 2.32 0.25 11.27 13.42 3.15 0.30 16.34 16.38 3.85 0.35 21.98 18.71 4.39 0.40 27.06 20.70 4.86