Research Article
Study on Long-Term Dynamic Mechanical Properties and Degradation Law of Sandstone under Freeze-Thaw Cycle
Figure 11
Failure modes of freeze-thaw cycle sandstone at 0.07 MPa impact pressure. (a) Typical failure patterns of a quarter of the specimen under numerical simulation. (b) Typical failure modes of laboratory test specimens.
(a) |