| Specimen designation | Liquid silicone rubber content (%) by total aggregates | Fine aggregate (%) | Coarse aggregate (%) | Superplasticizer to cement ratio (%) | Replicates of compressive test (at 28 days) |
| LF-G0S0 | 0 | 100 | 100 | 2 | 3 | LF-G1S1 | 1 | 99 | 99 | 2 | 3 | LF-G2S2 | 2 | 98 | 98 | 2 | 3 | LF-G4S4 | 4 | 96 | 96 | 2 | 3 | LF-G12.5S12.5 | 12.5 | 87.5 | 87.5 | 2 | 3 | LF-G25S25 | 25 | 75 | 75 | 2 | 3 | LF-G50S50 | 50 | 50 | 50 | 2 | 3 |
| HF-G0S0 | 0 | 100 | 100 | 2 | 3 | HF-G1S1 | 1 | 99 | 99 | 2 | 3 | HF-G2S2 | 2 | 98 | 98 | 2 | 3 | HF-G4S4 | 4 | 96 | 96 | 2 | 3 | HF-G12.5S12.5 | 12.5 | 87.5 | 87.5 | 2 | 3 | HF-G25S25 | 25 | 75 | 75 | 2 | 3 | HF-G50S50 | 50 | 50 | 50 | 2 | 3 |
|
|