Research Article
Metalized Plastic Waste Fiber Effects on Green Concrete Beams Mechanical Performance
Table 7
Compressive strength results (MPa).
| Mix | Days | 28 | 90 | 180 |
| Si7.5F0 | 34.6 | 36.3 | 38.9 | Si7.5F0.5 | 28.5 | 31.1 | 33.7 | Si7.5F1 | 26.3 | 28.1 | 31.2 | Si15F0 | 39.4 | 44.6 | 45.2 | Si15F0.5 | 30.3 | 33.4 | 36.8 | Si15F1 | 28.3 | 32.1 | 34.0 | Ze7.5F0 | 29.8 | 33.7 | 36.1 | Ze7.5F0.5 | 25.3 | 29.5 | 32.2 | Ze7.5F1 | 23.3 | 25.6 | 27.7 | Ze15F0 | 31.9 | 36.6 | 37.5 | Ze15F0.5 | 26.3 | 32.3 | 34.5 | Ze15F1 | 24.9 | 27.9 | 28.2 |
|
|