Research Article

The Importance of the Solids Loading on Confirming the Dielectric Nanosize Dependence of BaTiO3 Powders by Slurry Method

Table 1

The response sensitivity of to the under different solids loadings.

Given Δ %
( = 3000)( = 4000)

4%74.54774.6950.20
10%89.12789.6220.56
17%111.08112.291.09
25%145.27148.031.90