Research Article
Microstructural Evolution during DPRM Process of Semisolid Ledeburitic D2 Tool Steel
Figure 6
Microstructural development of AISI D2 after DPRM at 1300°C with a holding time of 5 minutes; (b) is the area within the black rectangle shown in (a).