The Scientific World Journal / 2013 / Article / Fig 9

Research Article

Damage Accumulation in Cyclically-Loaded Glass-Ceramic Matrix Composites Monitored by Acoustic Emission

Figure 9

Initiation frequency and strain versus time (a), duration and strain versus time (b), and RA and temperature versus time (c) for specimen B (notch-to-width 0.35).
869467.fig.009a
(a)
869467.fig.009b
(b)
869467.fig.009c
(c)