Research Article
The Effects of Salt on Rheological Properties of Asphalt after Long-Term Aging
Table 4
Failure temperature after PAV of SBS modified asphalt soaked in saline water.
| SBS modified asphalt | 0% 0 d | 0.3% 7 d | 0.3% 15 d | 1% 15 d | 1% 30 d | 3% 1 d | 3% 30 d | 5% 1 d | 5% 7 d |
| Failure temperature (°C) | 78.70 | 80.33 | 80.28 | 79.27 | 79.23 | 79.82 | 78.90 | 79.61 | 81.43 |
|
|