Effects of Processing Parameters on the Synthesis of (K0.5Na0.5)NbO3 Nanopowders by Reactive High-Energy Ball Milling Method
Figure 4
X-ray diffraction diagrams of as-milled (K0.5Na0.5)NbO3 prepared mechanochemically for (a) 5 h and (b) 10 h with the ball-to-powder mass ratio of 35/1 at 300, 400, 500, and 600 rpm.