Research Article
Impact Strength and Flexural Properties Enhancement of Methacrylate Silane Treated Oil Palm Mesocarp Fiber Reinforced Biodegradable Hybrid Composites
Table 1
PLA/PCL/clay/OPMF composition.
| Samples | PLA (g) | PCL (g) | Clay (g) | OPMF (g) |
| PLA/PCL/1 wt% clay/10 wt% OPMF | 22.72 | 4.01 | 0.27 | 3.00 | PLA/PCL/1 wt% clay/20 wt% OPMF | 20.20 | 3.56 | 0.24 | 6.00 | PLA/PCL/1 wt% clay/30 wt% OPMF | 17.67 | 3.1 | 0.21 | 9.00 |
|
|