Residual HEMA and TEGDMA Release and Cytotoxicity Evaluation of Resin-Modified Glass Ionomer Cement and Compomers Cured with Different Light Sources
Table 1
Composition of the resin modified glass ionomer cement and compomers used in this study.
| Materials | Organic matrix | Inorganic filler | (Filler content) | Size |
| Dyract Extra Lot#0809000332 Dentsply, USA | UDMA, carboxylic acid modified dimethacrylate resin, TEGDMA, BHT, strontium alimino-sodium-fluoro-silicate glass | Strontium fluoride glass particles | 50% volume | 0.8 μm |
| Twinkystar Lot#0919531 Voco, Germany | BisGMA, UDMA, TEGDMA, carboxylicacid modified methacrylate, camphorquinone, BHT | Barium aluminium fluorosilicate glass, strontium fluorosilicate glass, silicon dioxide | 77.8% w/w | 0.4–3.0 μm |