Research Article

Mineral Phases and Release Behaviors of As in the Process of Sintering Residues Containing As at High Temperature

Table 4

The As leaching concentration of sintered products for different sintering times.

Sintering time (min)HVEP (mg/L)TCLP (mg/L)

0(1)0.5680.751
50.4821.239
100.3170.554
150.1080.194
300.0860.0023
450.0030.0011
600.0020.0017
120n.d.0.0009

The specimen was not sintered.