Selected UPHC mixtures meeting the criteria for minimum required flow (180 mm) and 28-d compressive strength (150 MPa).

Mix IDFlow
(mm)
28-d
compressive
strength (MPa)
28-d flexural
tensile strength
(MPa)

BMWR23016131
NP60RMS19515429
FA60RMS21015832
LSP20RMS25515231
CKD20RMS22015225
PSS20RMS22516125
LSP10RSAND21516329
CKD05RSAND18015326
PSS05RSAND21016124
PSS10RSAND18515323
PSS20RSAND18016024