Heat Removal from Bipolar Transistor by Loop Heat Pipe with Nickel and Copper Porous Structures

Figure 3

Microscopic pictures of the sintered structures from nickel powders. (a) Grain size of 10 μm, sintering temperature of 600°C, and sintering time of 30 min. (b) Grain size of 25 μm, sintering temperature of 600°C, and sintering time of 30 min. (c) Grain size of 10 μm, sintering temperature of 600°C, and sintering time of 90 min. (d) Grain size of 25 μm, sintering temperature of 600°C, and sintering time of 90 min.
724740.fig.003a
(a)
724740.fig.003b
(b)
724740.fig.003c
(c)
724740.fig.003d
(d)

We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.