Porosity of sintered structures from nickel powder with grain size of 10 μm.

Grain size (μm)1010

Sintering temperature (°C)600600

Sintering time (min)3090

Porosity (%)6967

We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.