Experiment factors and ratios.
| Experiment factors | Levels |
| Fly ash replacement ratio | 0%; 15%; 25% | Water-binder ratio | 60%; 50%; 43% | Air content | ; | Durability improving admixture | 0 kg/m3; 10 kg/m3 |
|
|