Composition of the materials.

MaterialManufacturerCompositionFiller sizeLot numberShade

CompomerDyract eXtra (Dentsply DeTrey, Konstanz, Germany)Urethane dimethacrylate (UDMA), Carboxylic acid modified dimethacrylate (TCB resin), triethyleneglycol dimethacrylate (TEGDMA), trimethacrylate resin, camphorquinone, ethyl-4-dimethylaminobenzoate, butylated hydroxytoluene (BHT), UV stabiliser, strontium-alumino-sodium-fluoro-phosphor-silicate glass, highly dispersed silicon dioxide, strontium fluoride, iron oxide, and titanium dioxide pigments0.8  m11004002055A3

Nanofilled compositeNanosit (Nordiska Dental AB, Ängelholm, Sweden)Silanated barium glass, bisphenol A diglycidylmethacrylate (BisGMA), 1,6-hexanediol dimethacrylate, fumed silica, ethyl 4 dimethylaminobenzoate, camphorquinone, titanium dioxide, Dye (iron oxides), 2,4-dihydroxybenzophenone, and butylated hydroxyl toluene7 nm0510A3

Microhybrid compositeGradia Direct X (GC Co., Tokyo, Japan)Urethane dimethacrylate (UDMA), bisphenol A diglycidylmethacrylate (BisGMA), Fluoro-alumino-silicate glass, silica powder, prepolymerized filler, dimethacrylate, and camphorquinone0.85  m1104073A3

Nanofilled coatingG-Coat Plus (GC Co., Tokyo, Japan)Methylmethacrylate, multifunctional methacrylate, and camphorquinone35–40  m nanofiller particles0908061