Physicochemical characterization of PCHTs.
| CHT concentration (%) | Freezing temperature (°C) | Swelling ratio ( = 3) | Pore size (µm) ( = 20) | Porosity (%) ( = 3) | Young’s moduli (MPa) ( = 3) |
| 1 | −20 | 6.5 ± 0.4 | 425 ± 102 | 97.1 ± 0.3 | 0.037 ± 0.002 | 2 | −20 | 5.5 ± 0.9 | 418 ± 113 | 94.7 ± 0.8 | 0.5 ± 0.1 | 3 | −20 | 4.7 ± 0.9 | 336 ± 138 | 93.1 ± 0.5 | 1.1 ± 0.1 | 3 | −80 | 5.1 ± 0.9 | 2615 ± 60 | 91.7 ± 0.3 | 0.28 ± 0.01 | 3 | −196 | 6.4 ± 0.6 | 280 ± 6 | 92.5 ± 0.1 | 1.01 ± 0.05 |
|
|
Mean longitudinal size.
|