Research Article

Optimization and Prediction of Ultimate Tensile Strength in Metal Active Gas Welding

Table 1

Chemical compositions of base metal and electrode wire (% weight).

MaterialSSiMnCPFe

ST37-2 base metal0.0030.040.820.120.012Balance
ER70S-6 electrode0.010.581.150.080.014Balance