Research Article

Enamel Surface Damage following Debonding of Ceramic Brackets: A Hospital-Based Study

Table 4

Mean Adhesive Remnant Index among the different debonding techniques.

NMeanSt. deviationKruskal–Wallis χ2 value

US201.80000.4103915.080.002
DP202.60000.59824
LC202.00000.91766
TM202.40000.75394

Kruskal–Wallis test.