Research Article

Characterisation and Properties of Lithium Disilicate Glass Ceramics in the SiO2-Li2O-K2O-Al2O3 System for Dental Applications

Figure 3

The coefficient of thermal expansion of LD1, LD2, LD3, and LD4 which were heat-treated at 750–850°C for 2 hrs.
763838.fig.003