Mechanical Properties of Na2CO3-Activated High-Volume GGBFS Cement Paste

Table 3

Relative strengths of samples with the Na2CO3 activator compared to the strength of samples without activation.

Sample IDAge (d)Na2CO3 content (wt.%)
12345

R53114.98120.66125.17145.57147.85
7105.61119.28121.68125.13137.29
28103.62111.19117.80143.12158.88

R63112.07117.04122.83151.23128.96
7118.28119.64134.74152.14124.80
28113.36135.05153.53159.60156.40

R73105.93107.89134.02157.58145.22
7115.00118.75135.22147.86150.71
28108.62120.66136.61158.25163.63

R83103.06105.42126.21141.14164.29
789.6697.82120.26131.90154.34
2891.33108.71121.55139.43168.00

R93104.77109.94122.47129.75143.17
7100.00106.74119.21137.36144.83
28103.48105.49117.01133.86144.51

The results are listed relative to the strength of the sample without Na2CO3, which was considered to have a value of 100%.