Research Article
Effects of Doping Glass Fibers on the Early Strength of Sand-Based Cemented Paste Backfill for Solid Wastes Disposal in a Coal Mine
Table 4
Parameters of the slump testing of SCPB.
| Scheme | Glass fiber length (mm) | Glass fiber ratio (%) | Fly ash (%) | Aeolian sand (%) | Cement (%) | Quicklime (%) | Slump (mm) | Average (mm) |
| I | I1 | -- | -- | 47.5 | 39.5 | 8 | 5 | 261 | 269 | I2 | -- | -- | 47.5 | 39.5 | 8 | 5 | 276 | I3 | -- | -- | 47.5 | 39.5 | 8 | 5 | 271 |
| II | II1 | 6 | 1.0 | 46.5 | 39.5 | 8 | 5 | 207 | 209 | II2 | 6 | 1.0 | 46.5 | 39.5 | 8 | 5 | 214 | II3 | 6 | 1.0 | 46.5 | 39.5 | 8 | 5 | 208 |
|
|